Monel K-500 Producsts

Product Image (50)

Monel K-500 Pipe

  • Chemical Composition:Nickel-Copper alloy with small additions of aluminum and titanium
  • Density:8.44 Gram per cubic centimeter(g/cm3)
  • Hardness:High hardness due to age-hardening, Other
  • Material:Other, Monel K-500
  • Melting Point:1350–1390°C (2462–2534°F)
  • Resistance:Excellent corrosion and oxidation resistance
  • Tensile Strength:100000 to 110000 psi (typical)
  • Types of Alloy:Nickel-based alloy, Other
Product Image (51)

Monel K-500 Plate

  • Chemical Composition:Nickel-Copper Alloy
  • Density:8.44 Gram per cubic centimeter(g/cm3)
  • Hardness:Rockwell C40, Other
  • Material:Other, Monel
  • Melting Point:1350°C
  • Resistance:Corrosion and Alkali Resistant
  • Tensile Strength:965 MPa
  • Types of Alloy:Nickel-Copper Alloy, Other
Product Image (52)

Monel K-500 Sheet

  • Grade:Monel K-500
  • Material:Monel Alloy, Other
  • Product Type:Sheet
  • Resistance:Corrosion-resistant High-temperature-resistant
  • Shape:Other, Flat Sheet
  • Strength:High tensile and yield strength
  • Thermal Conductivity:Low
  • Thickness:Customizable
Product Image (53)

Monel K-500 Wire

  • Grade:Monel K-500
  • Material:Other, Monel K-500
  • Product Type:Wire
  • Resistance:Corrosion and oxidation resistant
  • Shape:Wire (coil form), Other
  • Strength:High strength and toughness
  • Thermal Conductivity:21 W/m·K
  • Thickness:Customizable based on requirements
Product Image (55)

Monel K-500 Fittings

  • Grade:Monel K-500
  • Product Type:Fittings
  • Shape:Other, Elbow Tee Reducer Coupling etc.
  • Strength:High strength with good ductility
  • Tensile Strength:900 MPa (approx)
  • Thermal Conductivity:21 W/m·K
  • Thickness:Standard as per fitting dimensions
  • Types of Alloy:Other, Nickel-based Alloy
Product Image (54)

Monel K-500 Rods

  • Color:Silver with Yellow End Caps
  • Grade:Monel K-500
  • Hardness:Brinell Hardness Test (Approximated), Other
  • Product Type:Rods
  • Shape:Other, Round Rod
  • Strength:High Strength with Enhanced Durability
  • Thermal Conductivity:21 W/m·K
  • Thickness:Customizable Based on Requirement