Inconel 600 Plate

  • Chemical Composition:Nickel-Chromium-Iron alloy
  • Density:8.47 Gram per cubic centimeter(g/cm3)
  • Grade:Inconel 600
  • Material:Other, Inconel
  • Product Type:Plate
  • Resistance:Excellent corrosion and oxidation resistance
  • Tensile Strength:655 MPa
  • Thermal Conductivity:15 W/m·K
Product Image (01)

Inconel 600 Pipe

  • Chemical Composition:Nickel-Chromium-Iron
  • Color:Silver
  • Density:8.47 Gram per cubic centimeter(g/cm3)
  • Hardness:Other, 88 HRB
  • Material:Other, Nickel Alloy
  • Product Type:Pipe
  • Resistance:Corrosion and Oxidation
  • Tensile Strength:655 MPa
Product Image (04)

Inconel 600 Sheet

  • Chemical Composition:Nickel 72% Chromium 14-17% Iron 6-10% Carbon <0.15% Manganese <1% Silicon <0.5% Sulfur <0.015%
  • Color:Silver Metallic
  • Grade:Inconel 600
  • Hardness:Other, 85 Rockwell B
  • Product Type:Sheet
  • Resistance:Corrosion and oxidation resistant
  • Tensile Strength:550 MPa
  • Thermal Conductivity:15 W/m·K
Product Image (02)

Inconel 600 Tube

  • Density:8.47 Gram per cubic centimeter(g/cm3)
  • Grade:Inconel 600
  • Material:Nickel-Chromium-Iron Alloy, Other
  • Melting Point:1370°C - 1425°C
  • Shape:Other, Cylindrical (Tube)
  • Strength:High mechanical strength
  • Thickness:Varies (commonly measured in mm)
  • Types of Alloy:Other, Superalloy (Ni-Cr-Fe)
Product Image (05)

Inconel 600 Wire

  • Chemical Composition:Nickel Chromium Iron
  • Color:Silver
  • Density:8.47 Gram per cubic centimeter(g/cm3)
  • Material:Inconel Alloy, Other
  • Product Type:Wire
  • Resistance:Excellent resistance to oxidation and corrosion
  • Tensile Strength:550 MPa (80 ksi)
  • Thermal Conductivity:15 W/m·K (at 100°C)
Product Image (06)

Inconel 600 Bar

  • Chemical Composition:Nickel 72% Chromium 14-17% Iron 6-10% Trace amounts of carbon manganese silicon sulfur and copper
  • Color:Silver
  • Grade:Inconel 600
  • Hardness:Other, 190-240 HB
  • Product Type:Bar
  • Resistance:Corrosion resistance in various environments and oxidation resistance
  • Tensile Strength:655 MPa
  • Thermal Conductivity:14.6 W/m·K at room temperature
Product Image (07)

Inconel 600 Fittings

  • Chemical Composition:Nickel-based Alloy (Ni Cr Fe)
  • Melting Point:1350°C - 1400°C
  • Resistance:Excellent resistance to oxidation corrosion and high temperatures
  • Shape:Various shapes (Elbow Tee Reducer etc.), Other
  • Strength:High strength at elevated temperatures
  • Tensile Strength:655 MPa (95 ksi)
  • Thickness:Varies based on specific fitting type
  • Types of Alloy:Other, High-performance Nickel-Chromium alloy