Hastelloy C276 Products

Product Image (29)

Hastelloy C276 Pipe

  • Hardness:Other, 85 HRB
  • Thermal Conductivity:9.8 W/mK
  • Tensile Strength:790 MPa
  • Melting Point:1350C - 1400C
  • Chemical Composition:Nickel Molybdenum Chromium Iron
  • Thickness:Varies as per specification
  • Types of Alloy:Nickel-Alloy, Other
  • Density:8.9 Gram per cubic centimeter(g/cm3)
Product Image (30)

Hastelloy C276 Tube

  • Thermal Conductivity:9.93 W/mK
  • Tensile Strength:750 MPa
  • Hardness:Approximately 87 HRB, Other
  • Melting Point:1325-1370C
  • Chemical Composition:Nickel-Molybdenum-Chromium alloy with Iron and Tungsten
  • Thickness:Variable (customizable based on application)
  • Types of Alloy:Other, Nickel-based alloy
  • Density:8.90 Gram per cubic centimeter(g/cm3)
Product Image (31)

Hastelloy C276 Plate

  • Product Type:Plate
  • Color:Silver
  • Resistance:Corrosion resistance to oxidizing and reducing agents
  • Types of Alloy:Other, Nickel alloy
  • Density:8.90 Gram per cubic centimeter(g/cm3)
  • Strength:High Strength
  • Shape:Other, Flat
  • Material:Hastelloy C276, Other
Product Image (32)

Hastelloy C276 Sheet

  • Density:8.90 Gram per cubic centimeter(g/cm3)
  • Types of Alloy:Other, Superalloy
  • Material:Other, Hastelloy
  • Shape:Other, Rectangular
  • Strength:High strength under stress
  • Grade:Hastelloy C276
  • Resistance:Corrosion-resistant
  • Product Type:Sheet
Product Image (34)

Hastelloy C276 Rod

  • Shape:Other, Round
  • Material:Hastelloy, Other
  • Strength:Good mechanical strength at high temperatures
  • Grade:C276
  • Density:8.89 Gram per cubic centimeter(g/cm3)
  • Types of Alloy:Other, Nickel Alloy
  • Resistance:Excellent resistance to corrosion stress corrosion cracking and pitting
  • Color:Silver
Product Image (35)

Hastelloy C276 Fittings

  • Thermal Conductivity:10.2 W/mK
  • Tensile Strength:790 MPa
  • Hardness:Other, 35 HRC
  • Melting Point:1370-1425C
  • Chemical Composition:Nickel-Molybdenum-Chromium-Iron
  • Thickness:Varies by product
  • Types of Alloy:Other, Nickel Alloy
  • Density:8.90 Gram per cubic centimeter(g/cm3)
Product Image (33)

Hastelloy C276 Wire

  • Chemical Composition:Nickel Molybdenum Chromium
  • Melting Point:1370C to 1425C
  • Hardness:Other, 95 HRB
  • Tensile Strength:690 MPa
  • Thermal Conductivity:9.8 W/mK
  • Thickness:Customizable
  • Material:Other, Nickel-Molybdenum-Chromium Alloy
  • Shape:Round Wire, Other