Back to top

Hastelloy C22 Products

Product Image (37)

Hastelloy C22 Tube

  • Chemical Composition:Nickel Chromium Molybdenum Iron
  • Density:8.69 Gram per cubic centimeter(g/cm3)
  • Grade:Hastelloy C22
  • Product Type:Tube
  • Resistance:Excellent Corrosion Resistance
  • Shape:Other, Cylindrical
  • Tensile Strength:690 MPa
  • Thickness:Customizable
Product Image (38)

Hastelloy C22 Plate

  • Chemical Composition:Nickel Chromium Molybdenum Iron
  • Density:8.69 Gram per cubic centimeter(g/cm3)
  • Grade:Hastelloy C22
  • Product Type:Plate
  • Resistance:Exceptional corrosion resistance against oxidizing and reducing environments
  • Shape:Other, Flat Sheet
  • Tensile Strength:690 MPa (100000 psi)
  • Types of Alloy:Other, Nickel-based Superalloy
Product Image (39)

Hastelloy C22 Sheet

  • Color:Silver
  • Hardness:Other, High
  • Material:Other, Hastelloy
  • Melting Point:1350–1400°C
  • Strength:High
  • Thermal Conductivity:9.2 W/m·K
  • Thickness:Varies
  • Types of Alloy:Other, Nickel-based
Product Image (40)

Hastelloy C22 Wire

  • Color:Silver
  • Hardness:Other, Rockwell B (RB) 90
  • Material:Hastelloy C22, Other
  • Melting Point:1320-1370°C
  • Strength:High strength and durability
  • Thermal Conductivity:8.9 W/m·K
  • Thickness:Customizable; typically 0.25mm to 5mm
  • Types of Alloy:Other, Nickel-based alloy
Product Image (41)

Hastelloy C22 Rods

  • Chemical Composition:Nickel Chromium Molybdenum Iron
  • Density:8.69 Gram per cubic centimeter(g/cm3)
  • Grade:C22
  • Hardness:Other, High
  • Product Type:Rod
  • Resistance:Corrosion Oxidation Pitting
  • Shape:Other, Cylindrical
  • Tensile Strength:690 MPa
Product Image (42)

Hastelloy C22 Fittings

  • Chemical Composition:Nickel Chromium Molybdenum and Iron
  • Density:8.69 Gram per cubic centimeter(g/cm3)
  • Grade:C22
  • Material:Other, Hastelloy
  • Product Type:Fittings
  • Resistance:Corrosion-resistant
  • Shape:Other, Elbow Tee Reducer Coupling
  • Tensile Strength:690 MPa
Product Image (36)

Hastelloy C22 Pipe

  • Color:Silver
  • Hardness:Other, Rockwell C 95
  • Material:Other, Hastelloy
  • Melting Point:1350°C - 1370°C
  • Strength:High strength and durability
  • Thermal Conductivity:9.3 W/m·K
  • Thickness:Customizable
  • Types of Alloy:Other, Nickel-based Alloy
X